100% satisfaction guarantee /Painters across metropolitan Adelaide

Preparation & Repairs

How to Fix Peeling Paint on Interior Walls

Find out why it peeled first, then scrape back to firm paint, feather the edges, seal the bare areas with a suitable primer and repaint. Skip the cause and it will peel again.

Neglected room with large sheets of pale blue paint peeling off the interior wall around a doorway

Peeling paint inside a house can be fixed for good, but only if you deal with the reason it peeled. The repair itself is straightforward: scrape off everything loose, sand the edges smooth, seal the exposed surface with the right primer and repaint. The part that gets skipped is working out what made the paint let go, and without that the new coat follows the old one onto the floor.

Common causes of peeling indoors

  • Moisture. Bathrooms, laundries and walls with plumbing behind them are the usual suspects. Steam or a slow leak gets behind the film and breaks the bond.
  • Painting over a dirty surface. Grease, soap residue and dust stop paint from gripping. Kitchens and hallways show this most.
  • Water based paint over old gloss. Many older homes have oil based enamel or gloss on walls and trims. Acrylic applied straight over it without sanding or an adhesion primer often peels in strips.
  • Powdery surfaces. Old distemper or soft, chalky paint in older homes gives new paint nothing firm to stick to.
  • New plaster that was never sealed. Topcoat applied directly to raw plaster can sit on the dusty surface layer and lift.
  • Salt damp. On the lower parts of masonry walls in older homes, salts pushing out of the wall cause bubbling and flaking.

A quick test helps. Press a strip of masking tape firmly onto the paint near the peeling area, then pull it off sharply. If paint comes away with it, the adhesion problem is wider than it looks.

Scraping back to a sound edge

Use a sharp scraper and work outward from the peeling area until the paint at the edge no longer lifts. Be thorough: anything that comes away easily now would have failed under the new coat anyway. Lay drop sheets first, and if the house was built before 1970, test for lead before scraping or sanding, because older layers may contain it.

Once the loose paint is off, wipe the area down to remove dust. If it is in a kitchen or bathroom, clean the surrounding wall properly too.

Feathering the edges

Where sound paint meets the bare patch there will be a ridge. Sand it with a block and 120 to 180 grit paper until the edge tapers smoothly into the surface below. On thick, layered paint you may not be able to sand it flat, in which case a thin skim of filler across the step, sanded once dry, gives a level surface. Shine a torch across the wall at a low angle to check: if you can see the outline, keep going.

Priming the repair

The primer is what stops the repair failing. Which one depends on the cause:

  • Bare plaster: a plaster sealer or sealer undercoat.
  • Chalky or powdery surfaces: a binding or penetrating primer that soaks in and locks the surface together.
  • Old gloss or enamel: a thorough sand and an adhesion primer suited to glossy surfaces.
  • Stains left behind by water: a stain blocking primer.

If you are unsure what primer does what, our article do you always need a primer explains the difference between primers, sealers and undercoats.

Repainting so it blends

Patching paint onto a single spot almost always shows. Even with matched colour, the sheen and texture of fresh paint differ from paint that has aged. For a result you will not notice, repaint the whole wall from corner to corner, using two coats over the primed repair. Check the tin for recoat times and keep a wet edge as you roll.

Stopping it happening again

Fixing the cause is the real repair. Run exhaust fans during and after showers, and make sure they actually vent outside. Get leaks repaired and give walls time to dry before painting. In wet areas, a finish made for bathrooms helps. On older masonry walls, persistent bubbling near the floor is often salt damp, which needs its own approach. Exterior paint peels for related reasons, covered in why exterior paint peels.

Peeling walls are a regular part of our interior painting work, and the site visit is where we work out what caused the failure before deciding how to put it right.

Keep reading

Related guides

All articles

Why Is My Exterior Paint Peeling?

Exterior paint peels when it loses its grip. The usual causes are moisture behind the paint, poor preparation, incompatible…

4 min read

How to Fill Cracks Before You Paint

Open the crack slightly, clean out the dust, fill with a product that suits the crack type, then sand flush and seal before…

4 min read

Free quotes

Want it done properly, first time?

Prefer to leave it to the professionals? We quote every job free, after a site visit.

Call us Free quote