100% satisfaction guarantee /Painters across metropolitan Adelaide

Preparation & Repairs

What Makes Paint Blister?

Paint blisters when heat or moisture pushes the film away from the surface. Painting in direct sun, damp substrates and water behind the wall are the usual causes. Fix the cause, then repaint.

Close-up of vertical timber boards with old cream paint cracking, lifting and flaking away to bare grey wood

Paint blisters when something pushes the film away from the surface underneath, forming raised bubbles. In Adelaide, the two usual culprits are heat and moisture. Heat blisters happen when fresh paint is applied in direct sun or onto a hot surface. Moisture blisters happen when water gets behind the paint, from damp timber, wet walls, leaks or rising damp. Working out which one you have tells you how to fix it and stop it coming back.

Heat blisters

When paint goes onto a hot surface, the outer skin dries very quickly. Solvent or water still trapped below then vapourises and has nowhere to go, so it lifts the soft film into small bubbles. This shows up most on:

  • North and west facing walls painted in the afternoon.
  • Dark colours, which absorb more heat.
  • Metal surfaces, such as gutters, fascias and doors, that get very hot in the sun.
  • Thick coats, or coats applied before the previous one had dried.

Heat blisters usually appear within hours or a day of painting. If you cut one open, you typically find paint underneath, not bare substrate. Our article on why you should not paint outside on a hot day explains how to work with the shade.

Moisture blisters

Moisture blisters can appear weeks, months or even years after painting, often after rain or in a particular season. The water comes from behind:

  • Timber that was damp when painted, or that soaks up water through unpainted end grain or gaps.
  • Leaks from gutters, roofs, flashings or plumbing.
  • Bathrooms and laundries, where steam moves through walls.
  • Masonry walls with rising or salt damp.
  • Walls painted too soon after pressure washing.

Cut one open and you will often find bare substrate, and sometimes water or dampness inside the blister. On older stone and brick homes, blistering in a band near the ground that returns after every repaint is a sign of salt damp, explained in salt damp in Adelaide homes.

Other causes worth knowing

  • Dirty or chalky surfaces can lead to poor adhesion, which allows blisters to form more easily.
  • Incompatible coats, such as some water based paints over old oil based enamel without preparation, can lose adhesion and lift.
  • Dew or rain on fresh paint before it has set can cause surface defects that look like blistering.
  • Solvent based paint in a closed, hot room can also blister if a coat is too heavy.

How to repair blistered paint

  1. Deal with the cause. Fix leaks, improve ventilation, or wait for cooler conditions. For damp walls, get the moisture sorted first.
  2. Scrape off the blisters. Remove all lifted paint back to a firm edge. If the house is old enough to have lead paint, test first and follow safe practices.
  3. Let the surface dry. Timber and masonry need time, especially after damp weather.
  4. Sand and feather. Sand edges smooth so the repair does not show a ridge, and lightly sand surrounding paint for adhesion.
  5. Prime bare areas. Use a primer suited to the substrate, such as timber primer or a masonry sealer.
  6. Repaint in the right conditions. Paint out of direct sun, on a surface that is not hot to touch, within the temperature range on the tin, and in coats that are not overly thick.

Stopping it next time

Most heat blisters are avoided by following the shade around the house: east walls in the morning, west walls later, and skipping painting on very hot days altogether. Moisture blisters are avoided by making sure the surface is dry before painting, sealing all sides and end grain of new timber, keeping gutters clear and fixing leaks quickly. Breathable coatings help on older masonry walls that hold some moisture.

Indoors, the same logic applies. Blisters in a bathroom ceiling usually mean steam is not being vented, while blisters low on a wall near a shower or a kitchen sink can point to a slow plumbing leak worth checking before repainting.

A blister is a message about what is happening under the paint, and reading it correctly is half the repair. On exterior painting jobs, we look at the pattern and timing of blistering during the site visit, deal with the cause where we can, and schedule work for the right times of day.

Keep reading

Related guides

All articles

Why Is My Exterior Paint Peeling?

Exterior paint peels when it loses its grip. The usual causes are moisture behind the paint, poor preparation, incompatible…

4 min read

How to Fill Cracks Before You Paint

Open the crack slightly, clean out the dust, fill with a product that suits the crack type, then sand flush and seal before…

4 min read

Free quotes

Want it done properly, first time?

Prefer to leave it to the professionals? We quote every job free, after a site visit.

Call us Free quote